Displaying welding circuit inductivity L
General The way that the interconnecting hosepack is arranged has a very significant effect on
the weld properties. In MIG/MAG pulse synergic welding in particular, high welding circuit
inductivity may occur, depending on the length of the interconnecting hosepack and the
way it is arranged. The current rise during droplet transfer is limited.
NOTE!
Wherever possible, compensation for the welding circuit inductivity is performed
automatically.
Where very high welding circuit inductivity occurs, it is also possible to attempt to influ-
ence the welding results with the droplet detachment correction parameter. If this does
not produce the desired result, you must rearrange the interconnecting hosepack.
Displaying weld-
ing circuit induct-
ivity L
1
Open the Setup menu level 2 (2nd)
2
Select parameter “L”
The welding circuit inductivity L calculated during the welding process is displayed
on the right-hand digital display.
L ... Welding circuit inductivity (in microhenrys)
Arranging the
interconnecting
hosepack cor-
rectly
Arranging the interconnecting hosepack correctly