The fixing conditions vary depending on the amount of pre-treatment solution used. The following
guidelines are approximate.
Note: If the pre-treatment solution is not completely dry after the suggested amount of time, extend the
duration while carefully checking if the pre-treatment solution is dry. If traces of the pre-treatment
solution are still visible, try using water to wash them off.
Application area size Temperature Time Pressure
Letter/A4 and smaller 338 °F (170 °C) 45 seconds 6 Psi
Larger than letter/A4 45–90 seconds
Note: Optimum conditions may vary depending on the type of heat press used; make sure to test in
advance to determine the correct conditions for your heat press.
Parent topic: Pre-treating a T-shirt
Preparing Your Printer
Before transmitting print data from the Garment Creator software, check the printer's status and make
sure that the print head nozzles are not clogged.
1. Turn on the printer.
35